Detail publikačního výsledku
Separation and preconcentration of platinum group metals and gold on modified silica and XAD sorbents in the presence of cationic surfactants for their determination by ICP-AES
Komendová, R., Sommer, L.
Originální název
Separation and preconcentration of platinum group metals and gold on modified silica and XAD sorbents in the presence of cationic surfactants for their determination by ICP-AES
Anglický název
Separation and preconcentration of platinum group metals and gold on modified silica and XAD sorbents in the presence of cationic surfactants for their determination by ICP-AES
Druh
Článek recenzovaný mimo WoS a Scopus
Originální abstrakt
Various modified silica sorbents and bare silica were tested for the separation and preconcentration of 10 - 200 ng cm-3 from 50 - 1000 cm3 sample volume of platinum group metals (PGMs), Pt(IV, II), Pd(II), Ir(IV), Rh(III), Os(VI), Ru(IV) and Au(III) in the form of ion associates of their chloro and bromo complexes with cationic surfactants. (1-(ethoxycarbonyl)pentadecyl) trimethylammonium bromide (Septonex®), benzyl(dodecyl)dimethylammonium bromide (Sterinol®), trimethyl(tetradecyl)- ammonium bromide and hexadecyl(trimethyl)ammonium chloride are suitable from 0.1 mol dm-3 HCl or 0.1 mol dm-3 HBr. A 100% recovery for Pd(II), Pt(IV) and Au(III) was obtained with octadecyl silicas Separon™ SGX C18, Separon™ SGX RPS and Phenyl™ silica in the presence of 0.006 mol dm-3 Septonex® or 0.003 mol dm-3 Sterinol®. The retained PGMs and Au(III) were eluted with acetonitrile and determined by inductively coupled plasma atomic emission spectrometry (ICP-AES) after evaporation of organic solvent in the presence of 0.1 mol dm-3 HCl. The enrichment factor on Separon™ SGX RPS reaches 100. A 1000: 1 excess of chloride, nitrate, sulphate, Na+, K+, Ca2+, Mg2+, Fe3+ or Al3+ does not interfere with the preconcentration of PGMs and Au(III) on this sorbent. With the silica-based anion exchanger Separon™ SGX AX the 100% recovery is observed for Ir(IV), Pd(II), Pt(IV) when the elution is performed with 5 mol dm-3 HCl or 5 mol dm-3 HNO3. Macroporous sorbents Amberlite™ XAD2 and Amberlite™ XAD4 are suitable for the retention of Au(III), Pd(II) and Pt(IV) from 0.1 mol dm-3 HCl and 0.006 mol dm-3 Septonex®. A 100% recovery is achieved by using acetonitrile as eluent but there is no preference of these sorbents to modified silica. In this way, the recovery of 0.1 - 0.2 ug cm-3 Au(III), Pd, Pt(IV) was also successfully tested with spiked matrices of soil extracts, power station dust samples and natural waters.
Anglický abstrakt
Various modified silica sorbents and bare silica were tested for the separation and preconcentration of 10 - 200 ng cm-3 from 50 - 1000 cm3 sample volume of platinum group metals (PGMs), Pt(IV, II), Pd(II), Ir(IV), Rh(III), Os(VI), Ru(IV) and Au(III) in the form of ion associates of their chloro and bromo complexes with cationic surfactants. (1-(ethoxycarbonyl)pentadecyl) trimethylammonium bromide (Septonex®), benzyl(dodecyl)dimethylammonium bromide (Sterinol®), trimethyl(tetradecyl)- ammonium bromide and hexadecyl(trimethyl)ammonium chloride are suitable from 0.1 mol dm-3 HCl or 0.1 mol dm-3 HBr. A 100% recovery for Pd(II), Pt(IV) and Au(III) was obtained with octadecyl silicas Separon™ SGX C18, Separon™ SGX RPS and Phenyl™ silica in the presence of 0.006 mol dm-3 Septonex® or 0.003 mol dm-3 Sterinol®. The retained PGMs and Au(III) were eluted with acetonitrile and determined by inductively coupled plasma atomic emission spectrometry (ICP-AES) after evaporation of organic solvent in the presence of 0.1 mol dm-3 HCl. The enrichment factor on Separon™ SGX RPS reaches 100. A 1000: 1 excess of chloride, nitrate, sulphate, Na+, K+, Ca2+, Mg2+, Fe3+ or Al3+ does not interfere with the preconcentration of PGMs and Au(III) on this sorbent. With the silica-based anion exchanger Separon™ SGX AX the 100% recovery is observed for Ir(IV), Pd(II), Pt(IV) when the elution is performed with 5 mol dm-3 HCl or 5 mol dm-3 HNO3. Macroporous sorbents Amberlite™ XAD2 and Amberlite™ XAD4 are suitable for the retention of Au(III), Pd(II) and Pt(IV) from 0.1 mol dm-3 HCl and 0.006 mol dm-3 Septonex®. A 100% recovery is achieved by using acetonitrile as eluent but there is no preference of these sorbents to modified silica. In this way, the recovery of 0.1 - 0.2 ug cm-3 Au(III), Pd, Pt(IV) was also successfully tested with spiked matrices of soil extracts, power station dust samples and natural waters.
Klíčová slova v angličtině
Platinum group metals; Gold; Sorbents; Modified silica; Amberlite XAD2 and XAD4; Quaternary ammonium surfactants; Inductively coupled plasma atomic emission spectrometry (ICP-AES)
Autoři
Komendová, R., Sommer, L.
Vydáno
01.01.2002
ISSN
0010-0765
Periodikum
Collection of Czechoslovak Chemical Communication
Svazek
67
Číslo
4
Stát
Česká republika
Strany od
454
Strany počet
17
Plný text v Digitální knihovně
BibTex
@article{BUT40872,
author="Renata {Komendová} and Lumír {Sommer}",
title="Separation and preconcentration of platinum group metals and gold on modified silica and XAD sorbents in the presence of cationic surfactants for their determination by ICP-AES",
journal="Collection of Czechoslovak Chemical Communication",
year="2002",
volume="67",
number="4",
pages="17",
issn="0010-0765"
}